Several misunderstandings in the processing of offset printing ink

In the film production process, it is often necessary to adjust the ink used appropriately. In order to meet the printing needs of different products and different papers. Adjust the ink appropriately. This is achieved by adding appropriate auxiliary materials to the ink. Because people have different understandings or prejudices on auxiliary materials, so. In actual production, it is likely to enter certain "misunderstandings" and produce unsatisfactory results.

1. Replace the ink adjusting oil completely with a debonding agent

during production. When printing a large-area field version. Ink is not easy to be evenly distributed in the process of ink roller transfer, or "paper fluffing" or roughness of printed products occurs Generally caused by the high viscosity of the ink.

Both the debonding agent and the adjusting ink can reduce the viscosity of the ink, but their properties are not exactly the same. The debonding agent has the effect of inhibiting the drying of the ink and reducing the adhesion of the ink layer to the paper while reducing the viscosity of the ink. Ink oil can reduce the viscosity of the ink and increase the fluidity of the ink in the ink. Although it can affect the drying speed of the ink layer, it is not obvious. If an excessive amount of debonding agent is added to the ink to reduce the viscosity of the ink, it is likely to cause "printing is not dry" or the ink layer is "pulverized". Therefore, we must pay attention to the "quantity" when adding the debonding agent, and we must not take it lightly. Keep it within the proper ratio. And at the same time increase the amount of desiccant. In order to avoid the above-mentioned adverse consequences.

2. Use white ink as diluent

Individual color inks need to add a diluent to the original ink to make it a light-colored ink, this diluent should have colorless and transparent properties. Both the brightening paste and the velvet oil are ideal impulsive agents. It has the effect of not changing the hue of the original ink but changing the depth of the original ink. If white ink is used as a diluent. Is inappropriate. Because white ink has a white hue, it will change the hue of the original ink so that the original ink tends to white and tender jade ink instead of becoming a light ink. This is contrary to the original intention of the operator to need light-colored ink. And in the offset printing process. If there are too many white ink components in the ink, due to the large proportion of white ink pigment particles, pigment particles will pile up on the printing plate or blanket during ink delivery. And cause the defects of rough imprint.

Third, do not distinguish between different works of anti-sticking agent and de-sticking agent

Adding anti-sticking agent to the ink can prevent or reduce the problem of sticking on the front and back of the printed paper. The degumming is to reduce the viscosity of the ink, it mainly plays its role in the process of ink transfer during printing. If the two are confused without distinction, it is likely that other problems will arise.

If a detackifier is added to the ink in order to prevent the ink on the front and back of the paper from sticking, the "non-dry" nature of the detackifier will prolong the drying time of the ink layer of the printed matter, which in turn makes the surface of the paper more sticky.

on the other hand. If more anti-blocking agent is added in order to reduce the viscosity of the ink in the printing process, it will not only play a good role in reducing the viscosity. It will also "roughen" the ink. Make it tarnish and affect the quality of the product.

Fourth, do not pay attention to the difference between red explosive oil and white explosive oil

Although red dry oil (also known as drilling dry oil) and white dry oil (also known as dry oil) are both desiccants for inks, they have different compositions. The drying form of the layer is also different.

Adding red dry oil to the ink can greatly accelerate the speed of oxidative film formation on the surface of the ink layer, that is, quickly dry on the surface of the ink layer. But red dry oil can't promote the dry operation speed inside the ink layer to be greatly improved. White oil has the performance of promoting the overall drying of the ink layer. When white ink is added to the ink, the drying speed of the surface and inside of the ink layer can be greatly improved. therefore. When we use desiccant. Attention must be paid to the difference between the two dry forms. E.g. For the drying of the ink layer surface. Red dry oil is better than white dry oil. However, in the case of a solid printing plate or paper with a thick printing ink layer, due to the relationship between acidity and alkalinity, the drying performance of the ink layer is not good. The surface is dry but the inside is not very dry. In the case of such a printed product, in the case of external friction, it is easy to wipe off the ink layer, leaving the printed product with scratches and affecting the quality of the product.

In addition, when printing gold ink, silver ink and need to add desiccant. Generally, red dry oil should be used instead of white dry oil. Because the combination of white dry oil and gold ink and silver ink. It has a tendency to make the original ink color darker. In this way, the printed product will affect the gloss effect of gold and silver ink.

Bathtub Length 1500-1800 MM

Drop in cast iron bathtubs are very popular. They're used in family bathrooms and hotels. The body of porcelain enamel cast iron bathtub is made of cast iron. And grade of porcelain enamel is A. Drop in bathtub also called build in bathtub, can be made in many different sizes and shapes. All drop in bath tubs are with legs and some items can be with handles.

drop in cast iron bathtubs 014

Bathtub Length 1500-1800 Mm,1800Mm Baths,Standard Bath Size,Freestanding Bath Tub

Anping Sunshine Sanitary Ware Co., Ltd. , https://www.sunshinebathtubs.com